Hits: 1646 img
In special sealing applications, ordinary silicone rubber suffers from insufficient oil resistance while fluororubber lacks low-temperature toughness. Extrudable fluorosilicone compound becomes an important elastomer that balances extrusion processability, oil & solvent resistance, and wide temperature adaptability. The 60 Shore A extrudable fluorosilicone compound is developed for continuously extruded sealing strips, hoses and profiled sealing parts. Many purchasers and process engineers often encounter pitfalls in material selection, vulcanization procedures and performance acceptance. This article focuses on processing guidelines, core performance parameters and selection tips for extrudable fluorosilicone compound.
1. What is extrudable fluorosilicone compound and what are its main advantages?
Extrudable fluorosilicone compound falls into the category of fluorosilicone silicone compound, specially formulated for extrusion molding and cured with matched peroxide vulcanizing agents. Compared with compression-molded fluorosilicone rubber, it is optimized for extrusion flowability and green strength after extrusion, while maintaining balanced mechanical strength and rebound performance. It inherits the excellent oil resistance, solvent resistance and wide-range temperature resistance of fluorosilicone materials, suitable for continuous production of rubber hoses, sealing strips and irregular profiled sealing profiles.
Key advantages:
2. Typical Performance Parameters of 60 Shore A Extrudable Fluorosilicone Compound
Note: Data in the table are typical lab values, not for final acceptance criteria. Heat-resistant additives can be compounded for more demanding heat resistance requirements.
| Test Item | Test Standard | Typical Value |
|---|---|---|
| Appearance | - | Light yellow, translucent |
| Density | ASTM D792 | 1.45 g/cm³ |
| Hardness (Shore A) | ASTM D2240 | 60 |
| Tensile Strength | ASTM D412 | 9 MPa |
| Elongation at Break | ASTM D412 | 320 % |
| Tear Strength | ASTM D624‑B | 20 KN/m |
| Compression Set (177℃, 22h) | ASTM D395 | 15 % |
| Rebound Resilience | ASTM D1054 | 25 % |
| Hardness Change after 200℃×72h Aging | ‑ | +3 Shore A |
| Tensile Strength Change after 200℃×72h Aging | ‑ | -20 % |
| Elongation Change after 200℃×72h Aging | ‑ | -20 % |
| Volume Change in Fuel C (25℃, 72h) | ASTM D471 | +20 % |
| Recommended Vulcanization Schedule | ‑ | 2phr Bis-2,4; Primary cure:120℃×15min, Post cure:200℃×4h |
3. What Should Be Prioritized for Material Selection and Incoming Inspection?
Hardness alone is not enough for selection. Process method, medium environment, temperature limit and compression set should be evaluated comprehensively.
4. Frequently Asked Questions
Q1: Can extrudable fluorosilicone compound and compression-molded fluorosilicone compound be interchanged?
A: Direct replacement is not recommended. Extrusion grades are optimized for flow, die swell and post-extrusion shape retention. Compression grades are designed for cavity filling, and tend to produce flash, rough surface and unstable dimensional tolerance on extrusion lines. Use dedicated extrusion grade for extrusion production.
Q2: Is Bis-2,4 the only available curing agent for this 60 Shore A grade?
A: No. The schedule listed is for reference only. Curing agent selection depends on extruder setup, part wall thickness and line speed. Bis-2,4 is widely used for extrusion, while other peroxide systems are also optional. Different vulcanizing agents will affect compression set and heat aging performance, and process validation is mandatory.
Q3: Does fluorosilicone rubber resist all types of oil?
A: Not exactly. It performs well with hydrocarbon fuel oils and certain mineral oils, but compatibility with ester oils and strong polar solvents needs separate immersion testing. Fuel C data only represents performance under that specific fuel condition. New working media require independent compatibility assessment.
Q4: Can post-curing be skipped? What are the consequences?
A: Post-curing is not recommended to be omitted for sealing parts. Post-curing removes volatile decomposition by-products from vulcanization, reduces compression set and improves thermal stability. Skipping this step will cause outgassing at high temperature, higher compression set and drastically shortened sealing service life.
Q5: Why do extruded profiles from different 60 Shore A fluorosilicone grades show obvious dimensional differences?
A: Hardness is just one parameter. Density, filler system, raw gum molecular weight and die swell effect all determine final dimensions. Die swell data must be reviewed for extrusion tooling, and die opening size should be adjusted according to swell coefficient instead of copying finished part dimensions directly.
Q6: Can higher post-curing temperature simply improve heat resistance of fluorosilicone compound?
A: Raising post-curing temperature alone brings limited benefits. To enhance long-term heat resistance, matched heat stabilizer formulation and standardized curing cycle are essential. Excessively high post-curing temperature will trigger thermal-oxidative degradation and reduce mechanical properties.
5. Summary Guidance for Material Selection
Fluorosilicone compound is a highly customized specialty elastomer. Hardness is only a basic reference. Five key evaluation factors should be considered: processing method, medium type, operating temperature (continuous vs peak), compression set and medium swelling rate. Sample trial validation before mass production helps reduce scrap and premature part failure.