Verification of Working Conditions and Raw Materials for High-Temperature HTV Silicone Rubber

Forming parameters shall be confirmed first before sample comparison. Good compounding performance does not guarantee that the elastic properties can be maintained after molding, extrusion and thermal aging. Room-temperature physical properties alone cannot represent the actual performance under long-term high-temperature service. During material selection, users shall provide forming parameters, post-curing schedule and target working conditions for review, followed by full validation by the end user.

This high-temperature resistant heat-vulcanized silicone rubber is suitable for compression molding and extrusion processes. For food-contact applications, finished parts require post-curing at 200°C for 4 hours.

Checklist for Verification

Category Details Inspection Focus of Test Specimens
Compounding & Vulcanization Curing agent type, dosage, vulcanization temperature, holding time, specimen thickness Curing completeness, surface condition, bubble formation, demoldability
Fabrication Process Compression / extrusion parameters, extrusion speed, die temperature, cooling setup Dimensional stability, surface finish, cracking and other defects
Post-Curing & Thermal Aging Post-curing temperature & duration, continuous operating temperature, aging cycle setting Hardness change after aging, retention of tensile strength, elongation and elasticity
Packaging & Storage Storage temperature, light protection, shelf life after opening, age from production date Plasticity variation, processing difficulty, vulcanization activity change

After switching to different hardness grades of high-temperature silicone rubber, mixing time, curing window and thermal aging performance must be re-evaluated. There is no universal process recipe directly applicable. Parameters shall be adjusted according to actual equipment conditions.

Typical Physical Properties

Note: Test specimen preparation: 0.6% DBPMH peroxide, compression cured at 175°C for 5 minutes, 2 mm sheet. Custom grades are excluded from this table and confirmation is required before customization.

Item HTV‑328‑40 HTV‑328‑50 HTV‑328‑60 HTV‑328‑70
Appearance Pale Yellow Pale Yellow Pale Yellow Pale Yellow
Williams Plasticity 150 200 240 240
Hardness (Shore A) 40 50 60 70
Density (g/cm³) 1.14 1.16 1.18 1.20
Tensile Strength (MPa) 8.5 9.0 9.5 9.0
Elongation (%) 700 600 500 400
Tear Strength (kN/m) 15 20 25 25
Hardness after 300°C × 72h aging 46 63 73 77
Tensile Strength after 300°C × 72h aging (MPa) 5.2 5.0 4.9 5.2
Elongation after 300°C × 72h aging (%) 350 220 180 160

This series is widely used for heat-resistant seals, extruded hoses and other components, balancing thermal resistance and fundamental mechanical performance.

How to Generate Valid Reference Data from Initial Sample Trials

  1. Select a reference material as benchmark, fix curing agent ratio, vulcanization temperature and duration. Record mixing behavior, demolding performance and surface quality.
  2. Produce parts with the target geometry. Once the forming process is stabilized, conduct thermal aging, sealing and mechanical reliability tests under agreed conditions. List uncertain working conditions as separate test items.
  3. Record batch number, storage environment and open-shelf duration. If abnormal performance occurs, repeat the full test sequence without changing multiple variables at once for easy troubleshooting.

High-temperature resistance, sealing reliability and food-contact compliance are separate acceptance criteria. Application description of the material does not automatically guarantee full compliance of finished products. It shall not be treated as a safety certification.

Samples and Technical Documentation

When sending an inquiry, please provide application, working temperature, forming technology, incumbent material system, failure symptoms and estimated order volume for material review. Custom grades require advance alignment on samples, test charges and lead time.

FAQ

Q1: Can this high-temperature HTV silicone rubber be directly used for food-contact products?

A: No. Material availability does not mean finished-part compliance. For food-contact applications, parts must undergo post-curing at 200°C for 4 hours, and pass relevant compliance testing before use.

Q2: Can grades with similar room-temperature properties replace each other directly?

A: Direct replacement is not recommended. Even if hardness and tensile data are close at ambient temperature, hardness and elongation retention differ significantly after long-term aging at 300°C. Mixing and curing windows also vary. Full validation under target conditions is mandatory.

Q3: Does stock exceeding the 3-month recommended usage window mean the compound is unusable?

A: Material is not automatically scrapped after 3 months, though extended mixing time may be needed. If you plan to use expired stock, recheck plasticity and post-cure mechanical properties to confirm fitness for production. From quality control perspective, use within 3 months is preferred. Unopened shelf life is 1 year from production in cool, dry and dark storage.

Q4: Does the 300°C × 72h aging data represent continuous service at 300°C all year round?

A: This is accelerated laboratory aging data for cross-reference only, not a lifetime guarantee. Actual service life is affected by pressure, oxygen atmosphere, chemical exposure and part thickness. Field reliability testing is required for real-life lifespan confirmation.

Q5: Can compression molding and extrusion share identical vulcanization parameters?

A: No. Heat transfer mechanisms differ between compression molding and extrusion. Wall thickness and line speed influence crosslinking degree. Curing and post-curing schedules must be tuned separately for each process.

Q6: Is choosing a higher Shore A grade sufficient when harder material is needed?

A: Hardness is only one indicator. Tear strength, elongation and retention after thermal aging must also be considered. Higher hardness grades feature lower original elongation and poorer retention after aging. Seal design requires comprehensive evaluation rather than hardness alone.

Q7: Can custom formulations refer to this standard property table?

A: This table applies only to standard grades. Modified custom compounds show different properties. Request the corresponding test report for custom grades before validation.


High Temperature Resistance Silicone Rubber(300℃),pls check IOTA HTV 328